Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-200L Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR .. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Middle Barrel Temperature | 241 - 254 °C | 466 - 489 °F | Injection Molding |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
LTL Color Compounds ColorFast® PBT100 PBT General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 241 - 254 °C | 465 - 490 °F | |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |