Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 238 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated
General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant
Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks
Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose
Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Ravago Manufacturing Americas Hybrid S459 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 238 - 260 °C
460 - 500 °F
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized
General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources NY6-IM1 Nylon 6, Impact Modified
Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized
Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 238 - 260 °C
460 - 500 °F
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Firestone C212-15C Nylon 6, Heat Stabilized
Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Firestone CL200-001 Nylon 6
Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Firestone CR212-203-D Nylon 6, Heat Stabilized
Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded
V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc.
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
LTL Color Compounds ColorFast® PBT100 PBT
General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc.
Middle Barrel Temperature 238 °C
460 °F
MTI ThermoStran® PP-30C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Middle Barrel Temperature 238 °C
460 °F
MTI ThermoStran® PP-40G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Middle Barrel Temperature 238 °C
460 °F
MTI ThermoStran® PP-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Middle Barrel Temperature 238 °C
460 °F
MTI ThermoStran® TPU-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Middle Barrel Temperature 238 °C
460 °F
MTI ThermoStran® TPU-60G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Middle Barrel Temperature 238 - 257 °C
460 - 495 °F
Diamond Polymers ASA/PC FA-30
Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Entec Hylox® 9015 PBT, 15% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Middle Barrel Temperature 238 - 254 °C
460 - 490 °F
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded
Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc.