Polymer Property : Middle Barrel Temperature = 480 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified
Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Ravago Manufacturing Americas Hybrid S459 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Firestone CL200-001 Nylon 6
Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Entec Hylox® 9020 PBT, 20% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 414 Polyester - PBT, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 415 Polyester - PBT, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 419 Polyester - PBT, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 421 Polyester - PBT, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Voloy® 411 Mineral Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Voloy® 415 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 462 Glass Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.