Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 227 - 238 °C | 440 - 460 °F | |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | >= 227 °C | >= 440 °F | |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Middle Barrel Temperature | 227 - 271 °C | 440 - 520 °F | |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Middle Barrel Temperature | 227 - 271 °C | 440 - 520 °F | |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Middle Barrel Temperature | 227 - 271 °C | 440 - 520 °F | |
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Middle Barrel Temperature | >= 227 °C | >= 440 °F | |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-200L Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 227 - 243 °C | 440 - 470 °F | |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Middle Barrel Temperature | 227 °C | 441 °F | |
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 227 - 254 °C | 440 - 490 °F | |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 227 - 271 °C | 440 - 520 °F | |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 227 - 271 °C | 440 - 520 °F | |
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 227 - 271 °C | 440 - 520 °F | |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |