Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 615 HP PET 15% Glass Reinforced Vypet VNT 615HP is a modified 15% fiberglass reinforced PET injection molding compound designed for automotive structural applications.Features: Easy, fast processing; Excellent strength and stiffne.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 930 PET 30% Glass Reinforced Vypet VNT 930 is a 30% fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityTypi.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 615 PET 15% Glass Reinforced Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYPET VNT 635A PET 35% Glass Reinforced Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 218W V15 PA66, 15% glass fiber, DRY Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: North AmericaProduct Applications: TECHNYL Â.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 258 PA Black 2N PA66, DRY Description: Unreinforced and modified polyamide 66, UV and thermal stabilized with excellent impact resistance, for injection molding.Available in: Europe Product Applications: TECHNYL® A 258P1 .. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY Description: High flow Polyamide PA66 Flame retarded grade reinforced with 30% glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applicat.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay Technyl® A218 Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay Technyl® A218GV33-BK 33% Glass Filled, Heat Stabilized, Hydrolysis Resistant, Black Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® AR 218 V33 Black 34 N Nylon 66, 33% glass fiber, DRY Description: Polyamide 66, reinforced with 33% of glass fiber, containing recycled material, for injection molding, specially stabilized to improve its resistance to automotive cooling liquids.Avail.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Feed Temperature | 250 - 270 °C | 482 - 518 °F | |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6 Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? G.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY Description: TECHNYL® AR 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled materials. This product is available in black .. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® SSD 330 KNF/E PA66, 15% glass filled, DRY Description: Polyamide 66, reinforced with 33% of glass fiber, for injection molding specially stabilized to improves its resistance to automotive cooling liquids.Available in: Asia PacificProduct A.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Feed Temperature | 265 - 270 °C | 509 - 518 °F | |
Solvay TECHNYL® 2710IR PA66, DRY Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.Benefits: This product, use.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Feed Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |