Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is suitable for automotive industry. This material is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
ISO 527 Type 1A
Elongation at Break 3.0 %
3.0 %
ISO 527 Type 1A
Tensile Modulus 11.0 GPa
1600 ksi
ISO 527 Type 1A
Flexural Modulus 9.20 GPa
1330 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
12.8 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C
505 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75/Af
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved