Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Unannealed; ISO 75-2/A |
PolyOne OnForce™ LFT NN-50LGF/000 HS Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Annealed 0.125 inch thick specimen; ASTM D648 |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | |
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | |
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | |
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/Af |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C @Thickness 3.20 mm |
491 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA LNP* LUBRICOMP* UFL36SXC is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA LNP* LUBRICOMP* UFL36SXQ is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15%PTFE. Added features of this material include: Wear Resistant, Heat Stabilized, Bearing Grade. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | GB/T 1634.2-2004 |
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C @Thickness 3.20 mm |
491 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/Af |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-2 |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON RE008 PA 66 LNP* STAT-KON* RE008 is a compound based on Nylon 66 containing 40% Carbon Fiber. Characteristics of this grade include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ASTM D648 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C @Thickness 3.20 mm |
491 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66 LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-2 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ASTM-D648 |
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/-2 |
DSM Akulon® S223-HG7 (Dry) 35% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30 Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Af |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-1/2 |
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Unannealed; ISO 75-2/A |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-2/AF |
Addiplast Addinyl A2 ZV30 Nylon 66, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75 |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |