Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648-95 |
Multibase Multi-Pro® 2005 T BLK Polypropylene PP compound suitable for automotive applications, meets elevated temperature resistance. Meets ESH-M4D-293-B specifications.Data provided by Multibase. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANLON A 5005B PA/ABS-Blend Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO data |
BASF Capron® 8202 NL Nylon 6 (Dry)
(discontinued **) Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
LyondellBasell SEQUEL® E3000 TPO Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C @Thickness 6.40 mm |
140 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUMID GP1300A(W) PA6, High Viscosity Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
Gromax CCP PBT 1100-211X Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9872105Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
Samyang Tribit® 1510 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1510 is a middle viscosity grade.Informatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | DIN 53461 |
Polyram PlusTek PB891 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75-93 |
Wellman Wellamid® XT1867-BK1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
Eastman Drystar 0827 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
Eastman Eastar EN010 Copolyester Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75-1/-2 |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | |
Aclo Accutech Polypropylene Copolymer HP0334W10L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336M10L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75 |
BASF Ultramid® 8202 HS BK-102 PA6 (Dry) Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75 |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM Test |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75-1/-2 |
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight develo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75 |
Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer Applications include injection molding and thermoforming. Antistatic stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM-D648 |
Braskem CP 404XP HECO Polypropylene Heterophasic Copolymer CP 404XP is a medium melt flow rate heterophasic copolymer with suitable additives to produce caps and closures for carbonated beverages. This product exhibits high stiffness and impact strength bal.. |