Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 0.965 g/cc
0.0349 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 10 %
10 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Flexural Strength 42.0 MPa
6090 psi
ASTM D790
Flexural Modulus 1.700 GPa
246.5 ksi
ASTM D790
Izod Impact, Notched 0.352 J/cm
0.660 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F