Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 1.925 GPa
279.2 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648