Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Unipetrol RPA
Trade Name PP MONSTEN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications include injection molding and thermoforming. Antistatic stabilized. Homopolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.0 MPa
5370 psi
ISO 527
Elongation at Break 80 %
80 %
ISO 527
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75
Vicat Softening Point 158 °C
316 °F
ISO 306