Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical with Impact = 149 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 5.99 mm
149 °F

@Thickness 0.236 in
UL 746
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
DSM Akulon® K224-HGR24 Nylon 6-30% Glass Fiber and Glass Bead Reinforced (European Grade) (Cond)  (discontinue
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.800 mm
149 °F

@Thickness 0.0315 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 65.0 °C

@Thickness >=3.00 mm
149 °F

@Thickness >=0.118 in
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity
Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 65.0 °C

@Thickness >=0.750 mm
149 °F

@Thickness >=0.0295 in
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Teknor Apex Chemlon® 253 Nylon 6, Toughened
Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation ..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
Eurostar Staramide AG6 PA66, 30% Glass Filled, Injection Molded
AG6 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded
AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded
BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL746B
DSM Akulon® K224-G0 (Dry) 50% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded
AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded
BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded
BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded
BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.400 mm
149 °F

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM
Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.400 mm
149 °F

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
DAM; UL 746B
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612  (Unverified Data**)
Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor..