Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Water Absorption 6.3 %
6.3 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 1.9 %
1.9 %
Humidity Absorption; Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa
26800 psi
ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
ISO 527-1/-2
Tensile Modulus 9.50 GPa
1380 ksi
ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
<br>@Temperature -30.0 °C
35.7 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
9.50 J/cm²
<br>@Temperature 23.0 °C
45.2 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
<br>@Temperature -30.0 °C
5.24 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
1.50 J/cm²
<br>@Temperature 23.0 °C
7.14 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
<br>@Temperature 20.0 °C
11.1 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 20.0 °C
38.9 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1/-2
UL RTI, Electrical 65.0 °C
<br>@Thickness 1.50 mm
149 °F
<br>@Thickness 0.0591 in
UL746B
65.0 °C
<br>@Thickness 0.750 mm
149 °F
<br>@Thickness 0.0295 in
UL746B
UL RTI, Mechanical with Impact 65.0 °C
<br>@Thickness 0.750 mm
149 °F
<br>@Thickness 0.0295 in
UL746B
65.0 °C
<br>@Thickness 1.50 mm
149 °F
<br>@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact 65.0 °C
<br>@Thickness 1.50 mm
149 °F
<br>@Thickness 0.0591 in
UL746B
65.0 °C
<br>@Thickness 0.750 mm
149 °F
<br>@Thickness 0.0295 in
UL746B
Flammability, UL94 HB
<br>@Thickness 1.60 mm
HB
<br>@Thickness 0.0630 in
IEC 60695-11-10
HB
<br>@Thickness 0.750 mm
HB
<br>@Thickness 0.0295 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.3
<br>@Frequency 1e+6 Hz
3.3
<br>@Frequency 1e+6 Hz
IEC 60250
3.5
<br>@Frequency 100 Hz
3.5
<br>@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Dissipation Factor 0.0050
<br>@Frequency 100 Hz
0.0050
<br>@Frequency 100 Hz
IEC 60250
0.015
<br>@Frequency 1e+6 Hz
0.015
<br>@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
>= 600 V
>= 600 V
PLC 0; UL 746A
Descriptive Properties Value Comments
Injection molding Yes
Release Agent Yes
With Fillers Yes