Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
STN EN 60695-2-12 |
Plastcom SLOVAMID® 6 GF 20 FRA 5 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 20% glass fiber, flame retarded with halogen flame retardant. Main features: flammability in accordance with UL 94 5 at 1.6 mm, glow wire at 960°C. Appli.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties for a wide variety of applications including business equipment, TVs, monitors, enclosures, among others.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANMID 6 B12^ NH6 Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANTEC PC S85R V0 Polycarbonate, Flame Retardant Information provided by Polykemi AB |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Glow Wire Test | 960 °C | 1760 °F | GWFI; IEC 695-2-1/2 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
PolyOne Bergadur™ PB40 G30 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Asia Pacific) Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Glow Wire Test | 960 °C @Thickness 0.800 - 3.00 mm |
1760 °F @Thickness 0.0315 - 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Glow Wire Test | 960 °C | 1760 °F | IEC 60695-2-12 |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
CEI 695 |
Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6 Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? G.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 695-2-1 |
Styron EMERGEâ„¢ 8600-10 Polycarbonate EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental .. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Glow Wire Test | 960 °C | 1760 °F | IEC 695-2-1 |
Supreme Petrochem SP 6456 High Heat Polystyrene Characteristics High heat resistance & strength Very good flow properties Available in any dark colorsProcessing Injection moldingApplications Instrument enclosures TV components Electrical encl.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East) |
|||
Glow Wire Test | 960 °C | 1760 °F | I.E.C. 695-2-12 |
Cossa Polimeri ESTABLEND PSA 8500 V0 HF Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, chlorine and bromine free, excellent light resistance, high impact resistance, excellent processabilityInformation pro.. |
|||
Glow Wire Test | 960 °C | 1760 °F | I.E.C. 695-2-1 |
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation.. |
|||
Glow Wire Test | 960 °C | 1760 °F | I.E.C. 695-2-1 |
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
Eurostar Starflam PX06020 PA6, Flame Retardant, Injection Molded Starflam PX06020 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
plaque; IEC 60695 |
Eurotec® Tecodur® PB70 GR15 NL TD 28 PBT 15% glass fiber reinforced, UL94 V0, impact modified, high CTI Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Glow Wire Test | 960 °C | 1760 °F | CEI 60695/2/1 |
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |