Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB SCANMID 6 B12^ NH6 Nylon 6, Flame Retardant, Halogen Free

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Polykemi AB
Trade Name SCANMID 6
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANMID 6 B12^ NH6 Nylon 6, Flame Retardant, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
With Flow; ISO 2577
0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 74.0 MPa
<= 10700 psi
ISO/R527
Elongation at Break 9.0 %
9.0 %
ISO/R527
Flexural Strength <= 115 MPa
<= 16700 psi
ISO 178
Flexural Modulus 3.00 GPa

@Temperature 23.0 °C
435 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
351 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
120°C/h; ISO 75/1
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
216 °C

@Load 1.00 kg
421 °F

@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
IEC 695-2-1