Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTACARB
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D 955
Melt Flow 8.0 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
8.0 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ASTM D 638
Elongation at Break 4.0 %
4.0 %
ASTM D 638
Flexural Modulus 3.50 GPa
508 ksi
ASTM D 790
Izod Impact, Notched 1.00 J/cm
<br>@Temperature 0.000 °C
1.87 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D 638
1.10 J/cm
<br>@Temperature 23.0 °C
2.06 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Hot Ball Pressure Test 135 °C
275 °F
I.E.C. 335-1
Vicat Softening Point 147 °C
<br>@Load 5.00 kg
297 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D 1525
150 °C
<br>@Load 0.999 kg
302 °F
<br>@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94 V-0
<br>@Thickness 1.60 mm
V-0
<br>@Thickness 0.0630 in
V-0
<br>@Thickness 3.20 mm
V-0
<br>@Thickness 0.126 in
Glow Wire Test 960 °C
1760 °F
I.E.C. 695-2-1
Copyright © lookpolymers.com All Rights Reserved