Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Annealed; ASTM D648 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ASTM D648 |
Kolon KOCETAL® GB705 Glass Bead Reinforced Acetal Resin Glass bead added, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | not annealed; ASTM D648 |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C @Thickness 3.20 mm |
325 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP KFI15 ACETAL LNP* LUBRICOMP* KFI15 is a compound based on Acetal containing 25% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C @Thickness 3.20 mm |
325 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer LNP* LUBRICOMP* KFL36 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C @Thickness 3.20 mm |
325 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High FlowInformation provided by .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass Fiber, 50% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C @Thickness 3.20 mm |
325 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP VERTON MVL36SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MVL36SX0 is a compound based on PP resin containing Long Glass Fiber and PTFE. Added features include: Chemically coupled, Heat Stabilized, Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75 |
Polyram RamTal PMH2003 Polyacetal Homopolymer for Injection Molding General purpose polyacetal homopolymer for injection molding applications, MFI 3.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75 -1 & -2 flat |
Asahi Kasei Tenac® 3013A Homopolymer Acetal Resin Weather-Resistant grade containing UV absorber and other additives for superior weathering abilityInformation provided by Asahi Kasei Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C | 325 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance. This black is formulated to mainta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 163 °C @Thickness 3.20 mm |
325 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |