Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON MVL36SX0 PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON MVL36SX0 PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* VERTON* MVL36SX0 is a compound based on PP resin containing Long Glass Fiber and PTFE. Added features include: Chemically coupled, Heat Stabilized, Internally Lubricated.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
Water Absorption 0.010 %

@Time 86400 sec
0.010 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0037 cm/cm

@Time 86400 sec
0.0037 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0073 cm/cm

@Time 86400 sec
0.0073 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 116 MPa
16800 psi
5 mm/min; ISO 527
Elongation at Break 2.2 %
2.2 %
5 mm/min; ISO 527
Tensile Modulus 8.50 GPa
1230 ksi
1 mm/min; ISO 527
Flexural Strength 133 MPa
19300 psi
2 mm/min; ISO 178
Flexural Modulus 6.50 GPa
943 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 42.0 kJ/m²
20.0 ft-lb/in²
80*10*4; ISO 180/1U
Impact Test 5.00 J
3.69 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af