Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Annealed; ISO 75-2A |
Total Lacqrene® 2551 Medium Impact Polystyrene
(discontinued **) LACQRENE® 2551 is a high heat resistance, medium impact polystyrene for injection molding. The very high Vicat Softening Point of this grade gives moldings of high rigidity and a good dimensional .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
LATI LASTIROL R G/30 30% Glass Fiber Reinforced Polystyrene (PS)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 12.7 mm |
201 °F @Thickness 0.500 in |
Unannealed; ASTM D648 |
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **) A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Load not specified; ASTM D648 |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ISO 75-1,-2 |
Ineos ABS Lustran® ABS 970 Lustran® ABS 970 has high impact strength and good paintability. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacomâ„¢ 63A6-4 Polypropylene Homopolymer Description: Hostacomâ„¢ 63A6-4 medium high melt flow, 2,200 MPa flexural modulus, 40% calcium carbonate-filled polypropylene homopolymer has an excellent combination of properties, chemical resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8004 FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8004 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8012 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8014 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 6.40 mm |
201 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 6.40 mm |
201 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® LX-0957 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C @Thickness 6.40 mm |
201 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ISO 75 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8002 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
Eastman Tritan MX731 Copolyester Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
Eastman Tritan TX1501HF Copolyester Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications Product Description: A homopolymer resin based on Exxpol™ metallocene technology designed for medical, electronics and other applications requiring cleanliness. It provides lower, volatiles and ext.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | 0.125";; ASTM D648 |
Diamond Polymers DIAMALOY GLY 9020 Sheet Extrusion Grade Diamaloy GLY 9020 resin is a high-gloss, low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
Braskem H 306 Fiber Extrusion Polypropylene Applications: Staple fibers for carpets and blankets. Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
Braskem H 306 Injection Molding Polypropylene Description: H 306 is a medium melt flow rate additivated homopolymer used for general purposes. It suitable for injection moulding and fiber extrusion. This product exhibits excellent processabilit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | Annealed, 1.8 Mpa;ASTM D648 |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |