Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® ABS 8012

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Techmer ES Plastiblend® ABS 8012.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 0.10 g/10 min
<br>@Load 3.80 kg,<br> Temperature 230 °C
0.10 g/10 min
<br>@Load 8.38 lb,<br> Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 33.8 MPa
4900 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
<br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
2.30 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature -40.0 °F
ASTM D256
1.82 J/cm
<br>@Thickness 3.17 mm,<br> Temperature 0.000 °C
3.40 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 32.0 °F
ASTM D256
4.48 J/cm
<br>@Thickness 3.17 mm,<br> Temperature 22.8 °C
8.40 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C
201 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
Unannealed; ASTM D648