Material Notes:
General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 5.6 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.6 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
19 g/10 min

@Load 10.0 kg,
Temperature 220 °C
19 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
Type I, 5 mm/min; ASTM D638
35.0 MPa
5080 psi
5 mm/min; ISO 527
Tensile Strength, Yield 44.0 MPa
6380 psi
Type I, 5 mm/min; ASTM D638
50.0 MPa
7250 psi
5 mm/min; ISO 527
Elongation at Break 24 %
24 %
Type I, 5 mm/min; ASTM D638
24.8 %
24.8 %
5 mm/min; ISO 527
Elongation at Yield 2.0 %
2.0 %
Type I, 5 mm/min; ASTM D638
2.6 %
2.6 %
5 mm/min; ISO 527
Tensile Modulus 2.27 GPa
329 ksi
5 mm/min; ASTM D638
2.53 GPa
367 ksi
1 mm/min; ISO 527
Flexural Yield Strength 72.0 MPa
10400 psi
1.3 mm/min, 50 mm span; ASTM D790
76.0 MPa
11000 psi
2 mm/min; ISO 178
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
2.41 GPa
350 ksi
2 mm/min; ISO 178
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
1.33 J/cm

@Temperature -30.0 °C
2.49 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 23.0 kJ/m²
10.9 ft-lb/in²
80*10*4; ISO 180/1A
8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Dart Drop, Total Energy 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 3.20 mm
201 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
80.0 °C

@Thickness 3.20 mm
176 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C
208 °F
Rate B/50; ASTM D1525
100 °C
212 °F
Rate B/50; ISO 306