| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.011 cm/cm | 0.011 in/in | MD; ASTM D955 |
| Melt Flow | 12 g/10 min | 12 g/10 min | ASTM D1238 |
| Ash | 10 % | 10 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 58 | 58 | ASTM D785 |
| Tensile Strength at Break | 15.0 MPa | 2180 psi | ASTM D638 |
| Tensile Strength, Yield | 22.0 MPa | 3190 psi | ASTM D638 |
| Elongation at Break | 40 % | 40 % | ASTM D638 |
| Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
| Tensile Modulus | 1.250 GPa | 181.3 ksi | ASTM D638 |
| Flexural Strength | 24.0 MPa | 3480 psi | ASTM D790 |
| Flexural Modulus | 1.100 GPa | 159.5 ksi | ASTM D790 |
| Izod Impact, Notched | 1.17 J/cm | 2.20 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F |