Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
Nylene® PA6/6 Homopolymer 132 HSL Nylon 6/6 Low Viscosity GP Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75/2Bf |
Radici Radilon® CARV300 L (dry) Copolyamide 66/6 Glass-fiber reinforcedInformation provided by Radici group. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75, ASTM D648 |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **) ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (Cond)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C @Thickness 6.40 mm |
455 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PET-RG20 Flame Retardant, 20% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66 Halogen free, Impact -resistantApplications A variety of connectorsInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET) Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66 LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOTUF VF004S PA 66 LNP THERMOTUF* VF004S is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Plastics Group Polifil® 628L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DIN 53461 |
Polyram PlusTek PA352M6 Nylon 6.6, 30% Low Friction Mineral Filled 30% low friction mineral filled polyamide 6.6 lubricated with molybdenum for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75 |
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | 0.455 MPa |
Toyobo ECOVYLOPET® EMC2310 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Unitika UNILATE® 1 SC PET Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DIN 53461 |
Polyram PlusTek RA103 Nylon 6.6, Impact Modified Impact resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
E-Polymers TEKAMID® TA210MS MoS2 Filled PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Clariant Renol PA111BK S&P Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75 |
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ashley Polymers Ashlene® 528LW Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Cheng Yu Plastic E2315 Flame Retardant PET, 15% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Toyobo Vylopet® EMC120K Glass Reinforced Polyester, Easy Molding Grade Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trackin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
Matrixx Group 80M7451 45% Glass/Mineral Filled PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |