Material Notes:
ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hrs.; ASTM D570
Water Absorption at Saturation 8.5 %

@Temperature 23.0 °C
8.5 %

@Temperature 73.4 °F
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 79
79
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 85.5 MPa
12400 psi
ASTM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Yield Strength 117.2 MPa
17000 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature -20.0 - 200 °C
45.0 µin/in-°F

@Temperature -4.00 - 392 °F
ASTM D696
90.0 µm/m-°C

@Temperature 93.3 - 238 °C
50.0 µin/in-°F

@Temperature 200 - 460 °F
ASTM D696
Maximum Service Temperature, Air 99.0 °C
210 °F
Long Term
179 °C
354 °F
Short Term
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 4.0

@Frequency 60 Hz
4.0

@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 11.8 - 15.7 kV/mm
300 - 399 kV/in
ASTM D149