Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Qualchem Danaprop PP1GF-30 Polypropylene, 30% Glass Fiber Polypropylene (co-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Quantum PBT Information provided by Quantum Advanced Engineering Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
LATI LATAN 23 Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 6.40 mm |
320 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Kolon KOCETAL® TC701 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 1-5830 30% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-5830 is a 30% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5830 is recommended for producing in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
Lanxess Pocan® B 7375 000000 PBT, White Pigment PBT, 25% white pigments, injection molding, improved light reflection, low tendency to warp |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
LATI Latene® AG7H2 G/50 PP Homopolymer, 50% Glass Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
LATI Latigray 82-03 CW/96 F3 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America;.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
LyondellBasell Higlass PF072-3 Polypropylene Homopolymer, 30% Glass Fiber Key Features: conventional melt flow, high modulus, chemically coupled, glass fiber-reinforced polypropylene homopolymer, high rigidity, high strength, good impact resistanceApplications: appliance .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS) Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO E TL20 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance and CopolymerProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 3.20 mm |
320 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 3.20 mm |
320 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 3.17 mm |
320 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® AC100-9 Acetal Copolymer Molding Resin Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461 |
Polyram RamTal PM7013 Acetal, UV Stabilized Polyacetal copolymer UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-30FG-0570 30% Glass Fiber Reinforced, Flame Retardant Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM Test |
BASF Ultramid® B50L 01 PA6 (Dry) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-25FG-0687 25% Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Ashley Polymers Ashlene® 851 Nylon 6, High Viscosity High viscosity for blown film, tubing, rods and shapes and blow molding. Has highest puncture resistance and clarity. FDA and NSF approved.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM HO TL20 BK Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 - 183 °C | 320 - 361 °F | Average value: 164 °C Grade Count:9 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |