Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 222 °C | 432 °F | ASTM D789 |
NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a gre.. |
|||
Melting Point | 222 °C | 432 °F | |
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® B 30 S FN40 000000 Nylon 6 PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1 |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYL® C 216 PA6, DRY Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
Melting Point | 222 °C | 432 °F | ISO 3146-C |
Solvay Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYL® C 502XT PA6, DRY Description: Unreinforced polyamide 6, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, shee.. |
|||
Melting Point | 222 °C | 432 °F | ISO 3146-C |
Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 30% GF, UV stabilized, for Injection molding. Available in: Europe and North AmericaProduct Applications: TECHNYLSTAR TM S 216L2 V30 BLACK is chara.. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Melting Point | 222 °C | 432 °F | |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BFZ 3 PA6 Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BG-30 PA6-GF30 Product description: Grilon BG-30 is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 has the following important properties: High stiffnessGood balance between stre.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BG-30 S PA6-GF30 Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BGK-30 X PA6-(GF+GB)30 Information provided by EMS Grivory |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® SK615SF BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF BK591 is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for i.. |
|||
Melting Point | 222 °C | 432 °F | ASTM D789 |
Adell BR-14 Nylon 6, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 222 °C | 432 °F | ASTM D3418 |
Ashley Polymers Ashlene® 833 Nylon 6 Basic Nylon 6 medium viscosity, with high residual monomer. Highly flexible and high strength, particularly suited for monofilament extrusion.Data provided by the manufacturer |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BRZ 334 H PA6 Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a.. |