| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Mineral Filled |
| Manufacturer | EMS-Grivory (EMS-CHEMIE) |
| Trade Name | Grivory® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | EMS-Grivory Grivory® BM-30/2 PA6-MD30.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
| Water Absorption | 7.0 % | 7.0 % | ISO 62 |
| Moisture Absorption | 2.00 % | 2.00 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 75.0 MPa | 10900 psi | conditioned; ISO 2039-1 |
| 180 MPa | 26100 psi | dry; ISO 2039-1 | |
| Tensile Strength, Yield | 50.0 MPa | 7250 psi | conditioned; ISO 527-1/-2 |
| 90.0 MPa | 13100 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 15 % | 15 % | dry; ISO 527-1/-2 |
| 15 % | 15 % | dry; ISO 527-1/-2 | |
| >= 50 % | >= 50 % | conditioned; ISO 527-1/-2 | |
| Elongation at Yield | 5.0 % | 5.0 % | dry; ISO 527-1/-2 |
| 25 % | 25 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 1.70 GPa | 247 ksi | conditioned; ISO 527-1/-2 |
| 5.00 GPa | 725 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 12.5 J/cm² | 59.5 ft-lb/in² | dry; ISO 179/1eU |
| 15.0 J/cm² | 71.4 ft-lb/in² | conditioned; ISO 179/1eU | |
| 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 12.5 J/cm² @Temperature 30.0 °C |
59.5 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | dry; ISO 179/1eA |
| 1.20 J/cm² | 5.71 ft-lb/in² | conditioned; ISO 179/1eA | |
| 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
| 160 °C | 320 °F | short term; EMS | |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 50.0 °C | 122 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | conditioned; IEC 60093 |
| 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | dry; IEC 60093 | |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Strength | 31.0 kV/mm | 787 kV/in | conditioned; IEC 60243-1 |
| 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 | |
| Comparative Tracking Index | 550 V | 550 V | conditioned; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive | Interior | |
| Form | Granules | |
| Industry & Consumer goods | Mechanical Engineering | |
| Tools & Accessories | ||
| Processing | Injection Molding |