Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Rynite® 940 NC010 PET
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Melting Point | 250 °C | 482 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Melting Point | 250 °C | 482 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Melting Point | 250 °C | 482 °F | |
Eastman Eastapak 7352 PET
(discontinued **) Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Melting Point | 250 - 258 °C | 482 - 496 °F | |
Isoflon Polyester film Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). .. |
|||
Melting Point | 250 °C | 482 °F | ISO 3146 |
Wellman Wellpet® GF100-BK1 PET, 30% Glass Fiber Reinforced Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division. |
|||
Melting Point | 250 °C | 482 °F | ISO 3146 |
Wellman Wellpet® GF100-N1 30% Glass Fiber Reinforced, Natural PET Description: Glass Fiber Reinforced, Natural PETInformation provided by Wellman. |
|||
Melting Point | 250 °C | 482 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1023CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1023CA is a metallocene ethylene-hexene copolymers. The slightly higher stiffness of Exceed 1023CA makes it easier to process on certain filling machinery, whilst still k.. |
|||
Melting Point | 250 - 260 °C | 482 - 500 °F | |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Melting Point | 250 - 260 °C | 482 - 500 °F | |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit.. |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Rynite® 940 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Melting Point | 250 °C | 482 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop.. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-HXGM24 PA410-(GF+MD)30 % Glass Reinforced, % Mineral Reinforced, Heat Stabilized |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 GR30 BK002 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | 10 K/min |
BASF Petra® 330 FR BK-112 30% Glass Filled PET Petra 330 FR BK-112 is a 30% glass reinforced, flame retardant PET, pigmented black injection molding compound rated UL94 V-0 in a 1/64 inch thickness. The product is designed for injection molding.. |
|||
Melting Point | 250 °C | 482 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Pocan® C 1206 000000 PET + PC PET + PC, non-reinforced, injection molding, improved impact strengthInformation provided by LANXESS. |
|||
Melting Point | 250 °C | 482 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Melting Point | 250 °C | 482 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |