| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eastman 7352 PET
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
| Bulk Density | 0.817 g/cc | 0.0295 lb/in³ | Poured; ASTM D1895 |
| 0.881 g/cc | 0.0318 lb/in³ | Vibrated; ASTM D1895 | |
| Density | 1.40 g/cc | 0.0506 lb/in³ | Crystalline Density; ASTM D1505 |
| Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
| Water Absorption | 0.10 % | 0.10 % | 24h Immersion; ASTM D570 |
| Particle Size | 2500 µm | 2500 µm | Pellet Size |
| Viscosity Measurement | 0.72 - 0.76 | 0.72 - 0.76 | Intrinsic; VGAS-A-AN-G-V-1 |
| Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 110 | 110 | ASTM D785 |
| Tensile Strength at Break | 26.0 MPa | 3770 psi | ASTM D638 |
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Flexural Yield Strength | 81.0 MPa | 11700 psi | ASTM D790 |
| Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
| Izod Impact, Notched | 0.360 J/cm @Temperature -40.0 °C |
0.674 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| 0.510 J/cm @Temperature 23.0 °C |
0.955 ft-lb/in @Temperature 73.4 °F |
ASTM D256 | |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
ASTM D4812 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | 63.0 J/g | 27.1 BTU/lb | ASTM E793 |
| Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
| 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 | |
| 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 | |
| 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 | |
| 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 | |
| Melting Point | 250 °C | 482 °F | Crystalline Peak Melting Point; ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 66.0 °C | 151 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
| Vicat Softening Point | 79.0 °C | 174 °F | 1kg load; ASTM D1525 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Surface Resistivity per Square | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 3.0 @Frequency 1e+6 Hz |
3.0 @Frequency 1e+6 Hz |
ASTM D150 |
| 3.2 @Frequency 1000 Hz |
3.2 @Frequency 1000 Hz |
ASTM D150 | |
| Dielectric Strength | 15.7 kV/mm | 399 kV/in | Short Time, 500V/sec; ASTM D149 |
| Dissipation Factor | 0.0080 @Frequency 1000 Hz |
0.0080 @Frequency 1000 Hz |
ASTM D150 |
| 0.020 @Frequency 1e+6 Hz |
0.020 @Frequency 1e+6 Hz |
ASTM D150 | |
| Arc Resistance | 155 sec | 155 sec | ASTM D495 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 275 - 295 °C | 527 - 563 °F | |
| Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
| Drying Temperature | 150 - 160 °C | 302 - 320 °F | |
| Dry Time | 4 - 6 hour | 4 - 6 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Acetaldehyde | <3ppm | VKCA-A-AS-G-GC-0001 |
| Color, CIE a* | -2.0 ± 1.5 | VGAS-A-AN-G-RS-001 |
| Color, CIE b* | 0.4 ± 1.5 | VGAS-A-AN-G-RS-001 |
| Color, CIE L* | 78.5 min | VGAS-A-AN-G-RS-001 |
| Fines, wt%, max | 0.05 | VGAS-A-AN-G-GA-1 |
| Pellet Shape | Cubical |