Material Notes:
Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containers used in the pharmaceutical industry. Voridian PET 5214A has Drug Master File No. 9987 filed with the U.S. FDA.Applications/UsesAutomotive parts containersFood packagingHousehold products containersPharmaceutical containersKey AttributesBrightTransparent
Physical Properties Metric English Comments
Bulk Density 0.817 g/cc
0.0295 lb/in³
Poured; ASTM D1895
0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.72 - 0.76
0.72 - 0.76
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 63.0 J/g
27.1 BTU/lb
ASTM E793
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
ASTM E1269
1.30 J/g-°C

@Temperature 80.0 °C
0.311 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.40 J/g-°C

@Temperature 100 °C
0.335 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.10 J/g-°C

@Temperature 280 °C
0.502 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 250 °C
482 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <3ppm
VKCA-A-AS-G-GC-0001
Color, CIE a* 3.3 ± 1.0
VGAS-A-AN-G-RS-001
Color, CIE b* 4.8 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE L* 45.3 ± 2.0
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.1
TEPO-A-AN-G-GA-4
Pellet Shape Cubical