Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 203 °F |
|
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP COLORCOMP DX98550H PC LNP* COLORCOMP* DX98550H is an unfilled Polycarbonate resin. Added features of this grade are: Low Extractable, Healthcare. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66 LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature 20.0 °C |
18.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
18.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
18.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RFB44XE PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB44XE is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature 20.0 °C |
18.3 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m.. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
18.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C | 18.3 µin/in-°F | ISO 11359 |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C | 18.3 µin/in-°F | ISO 11359 |
BASF Ultramid® A3EG3 BK00564 15% Glass Filled PA66 (Dry) Ultramid A3EG3 BK00564 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C | 18.3 µin/in-°F | ISO 11359 |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
18.3 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C | 18.3 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 33.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
18.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON RX00327 PA 66 LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural. |