Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer DuPont Performance Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance ofInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527-1/-2
Elongation at Break 2.2 %
2.2 %
ISO 527-1/-2
Tensile Modulus 6.135 GPa
889.8 ksi
ISO 527-1/-2
Flexural Strength 160 MPa
23200 psi
ISO 178
Flexural Modulus 6.00 GPa
870 ksi
ISO 178
Charpy Impact Unnotched 3.20 J/cm²
15.2 ft-lb/in²
ISO 179/1eU
2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ISO 179/1eA
0.600 J/cm²

@Temperature -40.0 °C
2.86 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 29.0 µm/m-°C
16.1 µin/in-°F
ISO 11359-1/-2
33.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
19.0 µm/m-°C

@Thickness 1.50 mm,
Temperature 55.0 - 160 °C
10.6 µin/in-°F

@Thickness 0.0591 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
52.8 µin/in-°F
ISO 11359-1/-2
74.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
41.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
125 µm/m-°C

@Temperature 55.0 - 160 °C
69.4 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
Melting Point 254 °C
489 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 238 °C
460 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.900 mm
V-0

@Thickness 0.0354 in
IEC 60695-11-10
5VA

@Thickness 1.50 mm
5VA

@Thickness 0.0591 in
IEC 60695-11-20
Descriptive Properties Value Comments
Part Marking Code >PET-GF15FR<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PET-GF15FR(17)
UL recognition UL