Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 92.8 °C | 199 °F | ASTM D1525 |
ExxonMobil LD 051.LT Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ASTM D1525 |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | 50°C/h 50N |
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ASTM D1525 |
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK12 is an SBC consisting of KR01 grade with a mold release added for easier processing. BK12 molded parts give excellent detail on fast production cyc.. |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B120; ISO 306 |
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5140 BLH is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-5140 BLH is recommended especially for producing products, where high stiffn.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ISO 306B |
Lucite International Diakon® LG156 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ISO 306 |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | ISO 306 |
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® WR-9160 ASA, Unreinforced Used in electric goods etc.Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | VST/B/50; ISO 306 |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 93.0 °C | 199 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL PX1007 PPE+PS Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade. |
|||
Vicat Softening Point | 93.0 °C @Load 5.10 kg, Temperature 50.0 °C |
199 °F @Load 11.2 lb, Temperature 122 °F |
ASTM D1225 |
Styrolution Terluran® EHI-4 NR ABS Extrusion Application Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 92.8 °C | 199 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRF 1707 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 93.0 °C | 199 °F | |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | |
Dow LDPE 993I Low Density Polyethylene DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability .. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | B50 (50N); ISO 306 |
Domo 1040SC Polypropylene Homopolymer Information provided by Domo. |
|||
Vicat Softening Point | 93.0 °C | 199 °F | |
BASF Novolen® 1102 G Polypropylene Data was collected by ISO methods and provided by BASF. |