Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It .. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® P36 Very High Flow Nylon 66 Description: Very high flowApplication: CompoundingInformation provided by NILIT. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® P50 Standard Viscosity Nylon 66 Description: Standard viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Vicat Softening Point | 255 - 263 °C | 491 - 505 °F | Average value: 262 °C Grade Count:14 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® P50FI Internally Lubricated Nylon 66 Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Carbon fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic.. |
|||
Vicat Softening Point | 255 °C | 491 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1/CF/30/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latigray 80-03 CWG/850 PPS, Glass/Metallic Reinforced Radiopaque compound based on Polyphenylene Sulfide (PPS). Metallic filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latiohm 66-05 PD01 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latiohm 80-05 CNT GCE/500 PPS, Glass/Mineral Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Carbon nanotubes. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Vicat Softening Point | 255 °C | 491 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR30 NL HW PA6.6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR35 NL HS PA6.6, 35% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |