Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PolyOne Maxxam™ DP-8928-2-1000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PTS Trilac® ABS-HS4000 General Purpose ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML6451 PC UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML6451 PC (Asia Pacific) UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ISO Value |
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose nylon 6 exhibiting excellent fluidity for filling thin sections. It possesses the combination.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
Firestone C212-15C Nylon 6, Heat Stabilized Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
Firestone CR212-203-D Nylon 6, Heat Stabilized Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear LNP LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing 45% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear (Asia Pacific) LNP* LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific) LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific) PPO/PS unfilled high heat |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific) Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. .. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific) LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |