Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 3.1 %
3.1 %
ASTM D638
Tensile Modulus 2.64 GPa
383 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.23
0.23
steel; ASTM D1894
Coefficient of Friction, Static 0.14
0.14
steel; ASTM D1894
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: