Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.30 GPa @Temperature 23.0 °C |
1350 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2mm/min; ASTM D790 |
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 (Asia Pacific) LNP LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFL26S PA 66 LNP* LUBRICOMP* RFL26S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFL26S PA 66 (Asia Pacific) LNP* Lubricomp* RFL26S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific) LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12 LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific) LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178-93 |
Wellman Wellamid® GF1758-BK2 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
Wellman Wellamid® GF33-66 22LH-N 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/15 42H-BKJA6A Nylon 6, 25% Mineral and 15% Glass Reinforced Ford JA6A color matchedAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ISO 178 |
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 246 SAN, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
Ascend Performance Materials VYDYNE® R533 Nylon, 33% Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Flexural Modulus | 9.30 GPa | 1350 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830L-33G Nylon 6, 33% Glass Reinforced A 33% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p.. |