Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.40 GPa | 1220 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 30 FRG 5 Polyamide 6, 30% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
PolyOne Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178-A |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon EE002ER PEI (Europe-Africa-Middle East) LNP* Lubricomp* EFP36G is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.This data wa.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | |
SPS Guang Zhou POBUXâ„¢ 3001G30 Flame-retarded/GF30%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PCN2615H PPE+PS (Asia Pacific) PPE+PS, Noryl, Glass Fiber, Mica, Flame Retardant, UL Grade, Non-Halogen Flame Retaardant, High Flow, |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | DAM; ISO 178 |
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Plenco 4327 Phenolic, Granular, Compression Molded PLENCO 04327 is a heat resistant mineral filled phenolic molding compound offering excellent cosmetic characteristics and improved heat resistant properties. PLENCO 04327 is not intended for electri.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Plenco 6582 Phenolic, Briquette, Injection Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178-93 |
Wellman Wellamid® MRGFX1716-BK1 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6 Description: Mineral/Glass Reinforced, Silicone Lubricated Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO 178 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
Ashley Polymers Ashlene® 541-33G Nylon 66, 33% Glass Reinforced Nylon 66, 33% glass reinforced for extrusion applications.Data provided by the manufacturer |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO Data |
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry) Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ISO Data |
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi.. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 623 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.40 GPa | 1220 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 610 Nylon 6, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |