BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 7.2 %
7.2 %
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
23°C/50% R.H.; ISO 62
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 120 MPa
17400 psi
5mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5mm/min; ISO 527
Tensile Modulus 9.30 GPa
1350 ksi
1mm/min; ISO 527
Flexural Strength 180 MPa
26100 psi
ISO Data
Flexural Modulus 8.40 GPa
1220 ksi
ISO Data
Izod Impact, Notched (ISO) 5.50 kJ/m²
2.62 ft-lb/in²
ISO Test
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179
5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ISO 11359
Melting Point 220 °C
428 °F
10 K/min
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.020

@Frequency 1.00e+6 Hz
0.020

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 400 V
400 V
IEC 60112
Descriptive Properties Value Comments
Color BK30564
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding