Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East) High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature -30.0 °C |
14.8 ft-lb @Temperature -22.0 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993... |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2X98703 ETFE LNP* THERMOCOMP* 2X98703 is a compound based on ETFE Copolymer resin containint Proprietary Filler(s). |
|||
Dart Drop, Total Energy | 20.0 J | 14.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 20.0 J | 14.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific) LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 20.0 J | 14.8 ft-lb | Total; ASTM D3763 |
Styrolution Styrolux® 3G46 SBC Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12 LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump.. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific) PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump .. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PX4605 PPE+PS PPE+PS blend. 20% Glass reinforced. High heat. Dimensional stability. Suitable for automotive and E/E applications. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2FL24 ETFE LNP* THERMOCOMP* 2FL24 is a compound based on ETFE resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is Wear Resistant. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific) PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate.. |
|||
Dart Drop, Total Energy | 20.0 J | 14.8 ft-lb | 1000N; ISO 7765-1 |
Borealis Borclear™ RE936CF Polypropylene Random Copolymer Borclear™ RE936CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: food packaging, lamination films, and stationary fil.. |
|||
Dart Drop, Total Energy | 20.0 J @Thickness 0.0500 mm |
14.8 ft-lb @Thickness 0.00197 in |
1000N; ISO 7765-2 |
Borealis Bormed™ RE806CF Polypropylene Random Copolymer Bormed™ RE806CF is a random copolymer. The material is specially formulated for medical applications. Applications: Bormed™ RE806CF is recommended for medical packaging. Bormed™ RE806CF contai.. |
|||
Dart Drop, Total Energy | 20.0 J @Thickness 0.0500 mm |
14.8 ft-lb @Thickness 0.00197 in |
1150N; ISO 7765-2 |
Borealis BorPure™ RD226CF Polypropylene Random Copolymer BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging.. |
|||
Dart Drop, Total Energy | 20.0 J | 14.8 ft-lb | 1150N; ISO 7765-2 |
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer BorPure™ RD266CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD266CF is recommended for
food packaging.. |
|||
Dart Drop, Total Energy | 20.0 J @Thickness 0.0500 mm |
14.8 ft-lb @Thickness 0.00197 in |
1150N; ISO 7765-2 |
Borealis BorPURE™ RE216CF Polypropylene Random Copolymer BorPure™ RE216CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: BorPure™ RE216CF is recommended for Lamination films, Me.. |
|||
Dart Drop, Total Energy | 20.0 J | 14.8 ft-lb | W<sub>501</sub> housing; ISO 6603-1 |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Dart Drop, Total Energy | 20.0 J @Temperature 23.0 °C |
14.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 3412ECR PC Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |