Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 45.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer
Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX2415 PC
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer
Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer
Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
conditioned; ISO 180-1U
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber
PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1U
Lanxess Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber
PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009. 30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber
SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 180/1U
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 180/1U
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded
Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 180/1U
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612  (Unverified Data**)
Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
DuPont Performance Polymers Crastin® LW9030 BK851 PBT  (Unverified Data**)
Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
conditioned; ISO 180-1U
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
Copyright © lookpolymers.com All Rights Reserved