Material Notes:
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D 792
Density 1.17 g/cc
0.0423 lb/in³
ASTM D 792
1.17 g/cc
0.0423 lb/in³
ISO 1183
Water Absorption 0.080 %
<br>@Time 86400 sec
0.080 %
<br>@Time 24.0 hour
ASTM D 570
Moisture Absorption at Equilibrium 0.13 %
0.13 %
23°C / 50% RH; ISO 62
0.13 %
0.13 %
50% RH; ASTM D 570
0.28 %
<br>@Temperature 23.0 °C
0.28 %
<br>@Temperature 73.4 °F
ASTM D 570
0.040 %
<br>@Time 86400 sec
0.040 %
<br>@Time 24.0 hour
50% RH; ASTM D 570
Water Absorption at Saturation 0.27 %
<br>@Temperature 23.0 °C
0.27 %
<br>@Temperature 73.4 °F
ISO 62
Moisture Vapor Transmission 0.900 cc-mm/m²-24hr-atm
<br>@Temperature 38.0 °C
2.29 cc-mil/100 in²-24hr-atm
<br>@Temperature 100 °F
100%RH; ASTM F 1249
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
Melt Flow 13 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
13 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
14.5 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
14.5 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 108
108
ASTM D 785
Hardness, Rockwell M 93
93
ASTM D 785
Hardness, H358/30 128 MPa
18600 psi
ISO 2039-1
Tensile Strength at Break 60.0 MPa
8700 psi
50 mm/min; ISO 527
65.0 MPa
9430 psi
Type I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 80.0 MPa
11600 psi
Type I, 50 mm/min; ASTM D 638
80.0 MPa
11600 psi
50 mm/min; ISO 527
Elongation at Break 40 %
40 %
50 mm/min; ISO 527
70 %
70 %
Type I, 50 mm/min; ASTM D 638
Elongation at Yield 7.0 %
7.0 %
Type I, 50 mm/min; ASTM D 638
7.0 %
7.0 %
50 mm/min; ISO 527
Tensile Modulus 2.45 GPa
355 ksi
1 mm/min; ISO 527
2.90 GPa
421 ksi
50 mm/min; ASTM D 638
Flexural Yield Strength 108 MPa
15700 psi
2 mm/min; ISO 178
120 MPa
17400 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.300 J/cm
<br>@Temperature 23.0 °C
0.562 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
0.300 J/cm
<br>@Temperature -30.0 °C
0.562 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
Izod Impact, Unnotched NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
<br>@Temperature -30.0 °C
1.90 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
5.00 kJ/m²
<br>@Temperature 23.0 °C
2.38 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
<br>@Temperature -30.0 °C
21.4 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1U
NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched 4.70 J/cm²
<br>@Temperature -30.0 °C
22.4 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
<br>@Temperature 23.0 °C
1.43 ft-lb/in²
<br>@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
0.300 J/cm²
<br>@Temperature -30.0 °C
1.43 ft-lb/in²
<br>@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Impact Test 30.0 J
<br>@Temperature 23.0 °C
22.1 ft-lb
<br>@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Taber Abrasion, mg/1000 Cycles 10
<br>@Load 1.00 kg
10
<br>@Load 2.20 lb
CS-17; ASTM D 1044
10
<br>@Load 1.00 kg
10
<br>@Load 2.20 lb
CS-17; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 95.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 203 °F
ASTM E 831
70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature -40.0 - 95.0 °C
38.9 µin/in-°F
<br>@Temperature -40.0 - 203 °F
ASTM E 831
70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ASTM C 177
0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Hot Ball Pressure Test <= 140 °C
<= 284 °F
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
268 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
133 °C
<br>@Thickness 3.20 mm
271 °F
<br>@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
244 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
119 °C
<br>@Thickness 3.20 mm
246 °F
<br>@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 138 °C
280 °F
Rate B/50; ISO 306
139 °C
282 °F
Rate B/50; ASTM D 1525
140 °C
284 °F
Rate B/120; ISO 306
Flammability, UL94 HB
<br>@Thickness 0.400 mm
HB
<br>@Thickness 0.0157 in
UL 94
Optical Properties Metric English Comments
Refractive Index 1.584
1.584
ASTM D 542
1.584
1.584
ISO 489
Haze <= 0.80 %
<br>@Thickness 2.54 mm
<= 0.80 %
<br>@Thickness 0.100 in
ASTM D 1003
Transmission, Visible 88 %
<br>@Thickness 2.54 mm
88 %
<br>@Thickness 0.100 in
ASTM D 1003
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
ASTM D 257
Dielectric Constant 2.8
<br>@Frequency 1.00e+6 Hz
2.8
<br>@Frequency 1.00e+6 Hz
ASTM D 150
2.9
<br>@Frequency 50.0 - 60.0 Hz
2.9
<br>@Frequency 50.0 - 60.0 Hz
ASTM D 150
Comparative Tracking Index 250 - 400 V
250 - 400 V
PLC code 2; UL 746A
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2
Erichson scratch depth, 6N, micrometer 14
SABIC Method
Pencil Hardness test, 1kgf H
ASTM D 3363
Copyright © lookpolymers.com All Rights Reserved