Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D 792 |
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
1.17 g/cc | 0.0423 lb/in³ | ASTM D 792 | |
Water Absorption | 0.080 % @Time 86400 sec |
0.080 % @Time 24.0 hour |
ASTM D 570 |
Moisture Absorption at Equilibrium | 0.13 % | 0.13 % | 23°C / 50% RH; ISO 62 |
0.13 % | 0.13 % | 50% RH; ASTM D 570 | |
0.28 % @Temperature 23.0 °C |
0.28 % @Temperature 73.4 °F |
ASTM D 570 | |
0.040 % @Time 86400 sec |
0.040 % @Time 24.0 hour |
50% RH; ASTM D 570 | |
Water Absorption at Saturation | 0.27 % @Temperature 23.0 °C |
0.27 % @Temperature 73.4 °F |
ISO 62 |
Moisture Vapor Transmission | 0.900 cc-mm/m²-24hr-atm @Temperature 38.0 °C |
2.29 cc-mil/100 in²-24hr-atm @Temperature 100 °F |
100%RH; ASTM F 1249 |
Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell L | 108 | 108 | ASTM D 785 |
Hardness, Rockwell M | 93 | 93 | ASTM D 785 |
Hardness, H358/30 | 128 MPa | 18600 psi | ISO 2039-1 |
Tensile Strength at Break | 60.0 MPa | 8700 psi | 50 mm/min; ISO 527 |
65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D 638 | |
Tensile Strength, Yield | 80.0 MPa | 11600 psi | Type I, 50 mm/min; ASTM D 638 |
80.0 MPa | 11600 psi | 50 mm/min; ISO 527 | |
Elongation at Break | 40 % | 40 % | 50 mm/min; ISO 527 |
70 % | 70 % | Type I, 50 mm/min; ASTM D 638 | |
Elongation at Yield | 7.0 % | 7.0 % | Type I, 50 mm/min; ASTM D 638 |
7.0 % | 7.0 % | 50 mm/min; ISO 527 | |
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
2.90 GPa | 421 ksi | 50 mm/min; ASTM D 638 | |
Flexural Yield Strength | 108 MPa | 15700 psi | 2 mm/min; ISO 178 |
120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 | |
Izod Impact, Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ASTM D 4812 |
Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A | |
Izod Impact, Unnotched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
80*10*3; ISO 180/1U | |
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
Impact Test | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
Taber Abrasion, mg/1000 Cycles | 10 @Load 1.00 kg |
10 @Load 2.20 lb |
CS-17; SABIC Method |
10 @Load 1.00 kg |
10 @Load 2.20 lb |
CS-17; ASTM D 1044 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 | |
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
70.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 | |
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 | |
Hot Ball Pressure Test | <= 140 °C | <= 284 °F | IEC 60695-10-2 |
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 268 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
133 °C @Thickness 3.20 mm |
271 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 244 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
Vicat Softening Point | 138 °C | 280 °F | Rate B/50; ISO 306 |
139 °C | 282 °F | Rate B/50; ASTM D 1525 | |
140 °C | 284 °F | Rate B/120; ISO 306 | |
Flammability, UL94 | HB @Thickness 0.400 mm |
HB @Thickness 0.0157 in |
UL 94 |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.584 | 1.584 | ASTM D 542 |
1.584 | 1.584 | ISO 489 | |
Haze | <= 0.80 % @Thickness 2.54 mm |
<= 0.80 % @Thickness 0.100 in |
ASTM D 1003 |
Transmission, Visible | 88 % @Thickness 2.54 mm |
88 % @Thickness 0.100 in |
ASTM D 1003 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D 257 |
Dielectric Constant | 2.8 @Frequency 1.00e+6 Hz |
2.8 @Frequency 1.00e+6 Hz |
ASTM D 150 |
2.9 @Frequency 50.0 - 60.0 Hz |
2.9 @Frequency 50.0 - 60.0 Hz |
ASTM D 150 | |
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC code 2; UL 746A |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |
Erichson scratch depth, 6N, micrometer | 14 | SABIC Method |
Pencil Hardness test, 1kgf | H | ASTM D 3363 |