Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 29.4 MPa @Time 86400 sec |
4270 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 29.4 MPa @Temperature 1100 °C |
4270 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 29.4 MPa @Time 86400 sec |
4270 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC90ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 29.4 MPa @Temperature 1300 °C |
4270 psi @Temperature 2370 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST SPL Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 29.4 MPa @Temperature 1100 °C |
4270 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST SUPER Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 29.4 MPa @Time 86400 sec |
4270 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics Smart Cast 9 Medium Cement Castables Information provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 29.4 MPa @Time 86400 sec |
4270 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 003 Smart Cast Application Special Properties: Anti-repellent PropertiesIndustry: CementApplication: Cement Plant Smoke ChamberInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 29.4 MPa @Temperature 110 °C |
4270 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 005 Smart Cast Application Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 29.4 MPa @Temperature 110 °C |
4270 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 009 Smart Cast Application Special Properties: Thermal Shock, Lesser Dross Formation, Non-wetting To AluminumIndustry: Non-FerrousApplication: Aluminum Melting/Holding Furnace, Launders, Risers, Transfer LaddlesInformation pr.. |
|||
Compressive Strength | 29.4 MPa @Temperature 1100 °C |
4270 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 29.4 MPa @Time 86400 sec |
4270 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 011 Smart Cast Application Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 29.4 MPa @Temperature 110 °C |
4270 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics ZAP 012 Smart Cast Application Special Properties: Patching At Hot Conditions, Easy InstallationIndustry: All IndustryApplication: All type of Rotary Kilns, AL/CU Melting Furnaces, Rolling Mills, Forgoing Furnaces, IncineratorsIn.. |
|||
Compressive Strength | 29.4 MPa @Temperature 500 °C, Time 10800 sec |
4270 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-120 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 110 °C, Time 86400 sec |
4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories BCT-130 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories BCT-145 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 110 °C, Time 86400 sec |
4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories BCT-145 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 110 °C, Time 86400 sec |
4270 - 5690 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CTL CGB-B Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 110 °C, Time 86400 sec |
4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTL-VBC Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 1500 °C, Time 10800 sec |
4270 - 5690 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 1000 °C, Time 10800 sec |
4270 - 5690 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 34.3 MPa @Temperature 1000 °C, Time 10800 sec |
4270 - 4980 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 1500 °C, Time 10800 sec |
4270 - 5690 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 110 °C, Time 86400 sec |
4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories SCX-70 I Special SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 1350 °C, Time 10800 sec |
4270 - 5690 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150S High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 110 °C, Time 86400 sec |
4270 - 5690 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150S High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175SV Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 1350 °C, Time 10800 sec |
4270 - 5690 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TPA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 29.4 - 39.2 MPa @Temperature 1500 °C, Time 10800 sec |
4270 - 5690 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |