| Category | Ceramic , Oxide , Silicon Oxide |
| Manufacturer | Chosun Refractories |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Chosun Refractories APC-120G Acid-proof Castable.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Rupture | 0.002943 GPa <br>@Temperature 110 °C,<br> Time 86400 sec |
0.4269 ksi <br>@Temperature 230 °F,<br> Time 24.0 hour |
|
| 0.006867 GPa <br>@Temperature 500 °C,<br> Time 10800 sec |
0.9960 ksi <br>@Temperature 932 °F,<br> Time 3.00 hour |
||
| 0.00981 GPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
1.42 ksi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
||
| Compressive Strength | 7.85 MPa <br>@Temperature 110 °C,<br> Time 86400 sec |
1140 psi <br>@Temperature 230 °F,<br> Time 24.0 hour |
Cold Crushing Strength |
| 24.5 MPa <br>@Temperature 500 °C,<br> Time 10800 sec |
3560 psi <br>@Temperature 932 °F,<br> Time 3.00 hour |
Cold Crushing Strength | |
| 29.4 MPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
4270 psi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
Cold Crushing Strength |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
| Shrinkage | -0.600 % <br>@Temperature 1000 °C,<br> Time 10800 sec |
-0.600 % <br>@Temperature 1830 °F,<br> Time 3.00 hour |
|
| -0.400 % <br>@Temperature 500 °C,<br> Time 10800 sec |
-0.400 % <br>@Temperature 932 °F,<br> Time 3.00 hour |
||
| -0.100 % <br>@Temperature 110 °C,<br> Time 86400 sec |
-0.100 % <br>@Temperature 230 °F,<br> Time 24.0 hour |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 42 % | 42 % | |
| SiO2 | 53 % | 53 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Installation Method | Spray | |
| Main Applications | Chemical Plant | |
| Material Required for Estimating (kg/?) | 2,200 |