| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Rupture | 0.005886 - 0.008829 GPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
0.8537 - 1.281 ksi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
|
| 0.005886 - 0.00981 GPa <br>@Temperature 1350 °C,<br> Time 10800 sec |
0.8537 - 1.42 ksi <br>@Temperature 2460 °F,<br> Time 3.00 hour |
||
| 0.005886 - 0.00981 GPa <br>@Temperature 110 °C,<br> Time 86400 sec |
0.8537 - 1.42 ksi <br>@Temperature 230 °F,<br> Time 24.0 hour |
||
| 0.007848 - 0.011772 GPa <br>@Temperature 1500 °C,<br> Time 10800 sec |
1.138 - 1.7074 ksi <br>@Temperature 2730 °F,<br> Time 3.00 hour |
||
| Compressive Strength | 29.4 - 39.2 MPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
4270 - 5690 psi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
Cold Crushing Strength |
| 34.3 - 39.2 MPa <br>@Temperature 1350 °C,<br> Time 10800 sec |
4980 - 5690 psi <br>@Temperature 2460 °F,<br> Time 3.00 hour |
Cold Crushing Strength | |
| 34.3 - 39.2 MPa <br>@Temperature 110 °C,<br> Time 86400 sec |
4980 - 5690 psi <br>@Temperature 230 °F,<br> Time 24.0 hour |
Cold Crushing Strength | |
| 44.1 - 53.9 MPa <br>@Temperature 1500 °C,<br> Time 10800 sec |
6400 - 7820 psi <br>@Temperature 2730 °F,<br> Time 3.00 hour |
Cold Crushing Strength |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 1.0817 W/m-K <br>@Temperature 260 °C |
7.4951 BTU-in/hr-ft²-°F <br>@Temperature 500 °F |
|
| 1.1515 W/m-K <br>@Temperature 540 °C |
7.9786 BTU-in/hr-ft²-°F <br>@Temperature 1000 °F |
||
| 1.2097 W/m-K <br>@Temperature 800 °C |
8.3816 BTU-in/hr-ft²-°F <br>@Temperature 1470 °F |
||
| Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
| Shrinkage | -0.200 % <br>@Temperature 1500 °C,<br> Time 10800 sec |
-0.200 % <br>@Temperature 2730 °F,<br> Time 3.00 hour |
|
| -0.100 % <br>@Temperature 1350 °C,<br> Time 10800 sec |
-0.100 % <br>@Temperature 2460 °F,<br> Time 3.00 hour |
||
| -0.0300 % <br>@Temperature 110 °C,<br> Time 86400 sec |
-0.0300 % <br>@Temperature 230 °F,<br> Time 24.0 hour |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 93 % | 93 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Installation Method | Casting | |
| Troweling | ||
| Material Required for Estimating(kg/?) | 2,850 | |
| Water Required for Casting(%) | 8.0 |