| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | Sharadaa Ceramics |
| Trade Name | Smart Cast |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Sharadaa Ceramics Smart Cast 9 Medium Cement Castables.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 2.35 g/cc | 0.0849 lb/in³ | After Drying at 110°C |
| Grain Size | <= 10000 µm | <= 10000 µm |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Rupture | 0.00000157 GPa @Temperature 110 °C |
0.000228 ksi @Temperature 230 °F |
|
| 0.00000167 GPa @Temperature 1100 °C |
0.000242 ksi @Temperature 2010 °F |
||
| 0.00000196 GPa @Temperature 1500 °C |
0.000284 ksi @Temperature 2730 °F |
||
| Compressive Strength | 123 MPa @Temperature 110 °C |
17800 psi @Temperature 230 °F |
Cold Crushing |
| 152 MPa @Temperature 1100 °C |
22000 psi @Temperature 2010 °F |
Cold Crushing | |
| 157 MPa @Temperature 1500 °C |
22800 psi @Temperature 2730 °F |
Cold Crushing | |
| 29.4 MPa @Time 86400 sec |
4270 psi @Time 24.0 hour |
Cold Crushing |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 1.49 W/m-K @Temperature 400 °C, Time 10800 sec |
10.3 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
| 1.63 W/m-K @Temperature 800 °C, Time 10800 sec |
11.3 BTU-in/hr-ft²-°F @Temperature 1470 °F, Time 3.00 hour |
||
| Maximum Service Temperature, Air | 1500 °C | 2730 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | >= 50 % | >= 50 % | |
| Fe2O3 | <= 1.1 % | <= 1.1 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Permanent Linear Change | -0.1 - 0.1% | 800 |
| -0.2 - 0.2% | 1100 | |
| -0.2 - 0.2% | 1500 | |
| Thermal Expansion | 0.5 | Reversible |
| Water Required to Mix | 4-5% |