Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.30 GPa | 769 ksi | |
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | |
Radici Radilon® A ERV3012 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527-2 |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Tensile Modulus | 5.30 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
769 ksi @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2/1 |
PolyOne Bergamid™ B70 GK/Mi30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527 |
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527 |
Nilit FRIANYL B63 L-HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527-1/-2 |
DSM Akulon® K224-PG2U (Dry) 13% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **)&l Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow) |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527-1/-2 |
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ZX89743 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZX89743 is a compound based on PPE+PS Blend resin containing Glass Fiber, Glass Beads and a Proprietary Lubricant. Added features include : Internally Lubricated. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East) LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF MF0049I PP (Europe-Africa-Middle East) LNP* THERMOTUF* MF0049I is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant, Chemically Coupled. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527-2 |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ASTM-D790 |
Polyram RamOfin PPH307G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | Film T.D.; ASTM D882 |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Tensile Modulus | 5.30 GPa @Temperature 200 °C |
769 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | ASTM D638 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15 Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s.. |
|||
Tensile Modulus | 5.30 GPa | 769 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo.. |