Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Polikim KESTOIL® Polyamide 6 + Lubricant Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ASTM D638 |
North Wood Plastics 60 PP + UNIFILL (40% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6) Information provided by PolyOne |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® APTIV® 2102-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled
(discontinued ** APTIV PEEK 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-2140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-2140 BLH is recommended especially for producing products, where high stiffness, low shrinkage, long term heat stability and excellent processability are required.All information pr.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Grupo Repol Dinalon® B1X25 V0 PA6 V0 Red Phosphorus and Halogen Free Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min; ISO 3268 |
Styron Pulse® 979 PC/ABS PULSE™ 979 is a high performance, 10% glass filled PC/ABS resin.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Polyram RamTough PZ305G4 Polycarbonate, 20% Glass Fiber 20% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
Corbion Purac Blend B High Heat, High Modulus Homopolymer PLA Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Increased modulus is produced by addition of talc to the base grade. Data is for samples.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
Covestro Makrolon® 8025 Polycarbonate High viscosity extrusion and injection molding grade with 20% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HB 5299 HV PA* Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ASTM D638 |
Ensinger XP-131 Compression Molded Unfilled PI The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber Contains 10% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black Information provided by Eurotec® |
|||
Tensile Modulus | 4.00 GPa @Temperature -40.0 °C |
580 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML3286 PC (Europe-Africa-Middle East) LEXAN ML3286 is a 17% glass reinforced grade for use in less demanding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527-1, 2 |
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Modulus | 4.00 GPa @Temperature 200 °C |
580 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |