Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Eurotec
Trade Name Tecomid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good chemical resistanceGood flow and processing propertiesAPPLICATIONS: AutomotiveElectrical/ElectronicFurnitureConstructionHome appliances
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Filler Content 0.00 %
0.00 %
ISO 3451
Moisture Absorption at Equilibrium 2.2 %
2.2 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 6.5 %
6.5 %
23°C; ISO 62
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
4.00 kJ/m²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 230 °C
446 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/2
Vicat Softening Point 245 °C
473 °F
50N; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 250 V
250 V
IEC 60112